Posted in

How to perform pre-heat treatment before welding?

When I first started in the heat treatment supply business over 12 years ago, I’d show up to job sites and watch welders grab their torches without a second thought about pre-heating. I’d see a steel fabricator in a rush, laying down a weld on a thick plate, and I’d know they were setting themselves up for trouble. Back then, I’d explain the science of pre-heating, and most would nod like they got it, but some would still skip it to save time. Now, after thousands of jobs, I don’t just tell them pre-heating is important—I show them why it’s non-negotiable, and I make sure they understand exactly how to do it right. This isn’t just about heating metal up; it’s a careful process that prevents cracks, improves weld quality, and saves you from costly rework later. Let me walk you through everything you need to know, from the basics to the fine details that most people miss. Heat Treatment

First, let’s get clear on what pre-heat actually is. It’s the practice of raising the temperature of the base metal before you start welding, holding that temperature for a set amount of time, and making sure the entire area where you’ll be welding is at that consistent temp. A lot of folks think it’s just “heating the metal so it’s not cold,” but that’s a myth. The goal is two-fold: one, to slow down the cooling rate of the weld and the surrounding base metal. When metal cools too fast after welding, it gets hard and brittle, especially in high-strength steels, carbon steels with more than 0.3% carbon, or alloys like chromium-molybdenum. That brittleness leads to cold cracks—those tiny, invisible fractures that can spread through the weld and cause a structure to fail months or years down the line. Two, pre-heat removes moisture that’s trapped in the base metal, especially in areas that might have rust, mill scale, or paint. Moisture breaks down when heated, releasing hydrogen that can get trapped in the weld metal and cause hydrogen-induced cracking, another common issue that’s hard to fix after the weld is done.

I see this mistake all the time: a welder uses a torch to warm up just the spot where they’re going to lay the first weld, and calls it pre-heat. That’s not enough. You need to heat a larger area—usually 3 to 6 inches around the joint, depending on the thickness of the metal. If you only heat the joint itself, the edges of the base metal are still cold, so when you weld, the heat from the torch gets sucked out of the weld pool too fast, leading to uneven cooling and more stress. For thick metal plates, say 2 inches or more, that heating area needs to be even bigger—up to 8 inches out—because thick metal holds more cold, so the heat has to spread further to make a consistent temperature.

Now, how do you figure out what the right pre-heat temperature is? That’s where the science comes in, and it’s not one-size-fits-all. The main factors are the type of base metal, its thickness, the welding process you’re using, and the final service conditions of the structure you’re building. For example, carbon steel with a carbon content below 0.25% usually only needs a low pre-heat, around 50 to 100 degrees Fahrenheit, but if that same steel is over 1 inch thick, you’ll need 150 to 200 degrees. High-strength steels, like those used in bridges or heavy equipment, often require 300 to 500 degrees, and some specialty alloys need even more. I always tell customers to check the material’s data sheet first—most mills specify the minimum pre-heat temperature, and that’s your starting point. Never go lower than that, even if you’re in a hurry. I once had a customer who skipped pre-heat on a 1.5-inch A36 steel weld, and three weeks later, the inspector found a crack that ran all the way through the weld. They had to cut out the entire weld, re-pre-heat the joint, and redo the whole job—cost them 10 times what a proper pre-heat service would have. That’s the kind of mistake you can’t afford to cut corners on.

Next, how do you actually apply the pre-heat? There are a few methods, and each has its place. Torch heating is the most common, especially for small jobs, but it’s also the hardest to get consistent temperatures with. If you’re using a torch, you have to move it slowly and evenly around the area, not focus on one spot too long or you’ll burn the metal. You also need to measure the temperature as you go—just guessing is a bad idea. That’s where temperature indicators come in: crayons that melt at a specific temp, or non-contact infrared thermometers. I recommend both. Crayons are cheap and reliable for on-site work, and they give you a visual mark that the area has reached the right temp. Infrared thermometers are good for checking multiple spots, especially on large structures. But here’s a tip: the temperature you measure with a non-contact tool is the surface temp. To get the core temp, you need to let the metal stabilize for a few minutes after heating—thick metal will take longer to heat through, so don’t start welding right after you see the surface hit 300 degrees.

For bigger jobs, like pipe welding or large structural steel, induction heating is a game-changer. Induction uses electromagnetic coils wrapped around the joint, which heat the metal evenly from the inside out. No open flames, so it’s safer around flammable materials, and you can maintain a consistent temp across the entire area. I’ve used induction heating on 12-inch thick steel plates for a power plant project, and it cut the pre-heat time in half compared to torch heating, with way less uneven temperature spots. Another option is resistance heating, where you run a low-voltage current through the metal, heating it uniformly. That’s great for thin sheets or small parts, where torch heating might warp the metal.

One step most people forget is holding the pre-heat temperature. It’s not enough to bring the temp up to the right number and then start welding. You need to keep it there for a set amount of time—usually 1 to 5 minutes, depending on thickness. This gives the moisture trapped in the metal time to evaporate, and it ensures the entire joint stays at a consistent temp so when you weld, the cooling rate is slow and even. If you heat to 300 degrees, then start welding immediately, the metal will start cooling before you’re done, and you’ll get that fast cooling that causes cracks. I always make sure to remind customers: “Heat it, hold it, then weld it—not heat it and jump into it.”

What about post-heating, you might ask? That’s related, but pre-heating is the foundation. Post-heating is heating the weld after it’s done, usually to relieve stress, but pre-heat works before you even strike the arc to prevent problems from the start. You can’t skip pre-heat and rely on post-heat to fix everything—they work together, but pre-heat is the first line of defense.

I want to talk about a common misconception when working outdoors. If you’re welding in cold weather, say below 50 degrees, you need to bump up the pre-heat temperature by 50 to 100 degrees. The cold air will suck heat out of the metal fast, so your pre-heat has to be higher to compensate. I had a customer last winter who was welding a steel frame outside, and they only did the standard 100 degrees pre-heat. The wind was blowing at 20 mph, and by the time they finished the weld, the metal was already down to 50 degrees. They ended up with 30% of their welds cracking within a month. We went back and re-pre-heated those joints with 200 degrees and wind barriers, and the problem went away. Wind or low temperatures don’t just change the pre-heat number—they change how you apply it. If you’re working outside, use wind screens to keep the heat from blowing away, and make sure you account for the ambient temp when calculating your pre-heat.

Another thing to watch for is dissimilar metal welding. If you’re welding two different metals, like carbon steel to stainless steel, the pre-heat requirements get more complicated. The different metals have different thermal expansion rates, so uneven heating can cause stress that leads to cracks. You might need to pre-heat to a temperature that’s a middle ground between the two metals’ requirements, or even use a different method like induction heating to keep the temperature consistent across both. I always suggest testing a small sample joint first when dealing with dissimilar metals—way better than messing up a big, expensive structure.

Now, let’s talk about how as a heat treatment supplier, we make this process easier for our customers. A lot of fabricators don’t have the equipment or expertise to do pre-heating correctly, especially on large or complex jobs. We don’t just show up with a torch or an induction coil—we do a site assessment first. We look at the material specs, the thickness, the joint design, the ambient conditions, and the welding process planned. Then we recommend the right pre-heat method, set the temperature, and monitor the entire process from start to finish. We provide temperature logs that you can show to inspectors, which is a big deal for projects that require documentation. I’ve had customers tell me that the inspector passed their welds with no issues, and that’s because we did the pre-heat right. We also have the equipment to handle any job, from small pipe fittings to 20-inch thick structural plates, so you don’t have to rent multiple tools or figure out how to use them.

I always tell my clients that pre-heating isn’t an expense—it’s an investment. The cost of rework, delays, and structural failures way outweighs the cost of a proper pre-heat service. I’ve seen jobs where a $500 pre-heat job saved a $50,000 weld rework, and that’s not an exaggeration. Cracks in welds don’t just cost money to fix—they can delay projects, hurt reputations, and even create safety hazards. Pre-heating is a simple step that prevents all that.

Let me share a recent example to drive this home. A local construction company was working on a new bridge, and they had a 1.75-inch thick A572 Grade 50 steel joint that needed to be welded. Their in-house crew tried to pre-heat it with torches, but they were only heating a 2-inch area around the joint, and they only held the temp for 30 seconds. Halfway through the welding, the inspector noticed tiny cracks forming. They called me, and we re-pre-heated the joint with induction heating, heating a 6-inch area to 350 degrees and holding it for 5 minutes. The welds went in smooth, no cracks, and the bridge was completed on time. That company could have saved themselves a lot of stress and time if they’d done it right the first time.

So, to wrap this up, here’s your step-by-step guide to pre-heating before welding:

First, identify your base metal, its thickness, and the required pre-heat temperature from the material data sheet. If you’re working in cold weather or outdoors, adjust that temp upward by 50-100 degrees and set up wind protection.

Next, choose your heating method: torch for small jobs, induction or resistance for large, consistent jobs. Make sure you’re heating the required area—3-8 inches around the joint, depending on thickness.

Then, heat the area until it reaches the correct temperature, and use temperature indicators (crayons, thermometers) to verify across the entire heating zone. Hold that temperature for the required time (1-5 minutes, more for thicker metal) to let moisture evaporate and the heat spread through the base metal.

Finally, start welding immediately after holding the temp. Don’t let the metal cool down before you begin, and keep track of the weld temperature as you go to make sure it stays consistent.

If this sounds like more than you want to handle on your own, we’re here to help. We’ve got the experience, equipment, and expertise to get your pre-heating right every time, so you can focus on getting the welds done correctly and keeping your project on track. We provide on-site heat treatment services, customized solutions for any type of metal or job, and detailed documentation to keep your inspectors happy. To learn more about how we can support your welding projects with professional pre-heat treatment, reach out to us to discuss your needs.

Auto Forks References

  1. American Welding Society. (2018). AWS D1.1: Structural Welding Code – Steel.
  2. ASM International. (2008). Heat Treater’s Guide: Practices and Procedures for Irons and Steels.
  3. British Standards Institution. (2019). BS EN 1011-2: Welding – Recommendations for welding of metallic materials – Part 2: Arc welding of ferritic steels.
  4. Lincoln Electric. (2020). Welding Fundamentals: Preheating and Postheating of Steels.

Ningbo Bolong Machinery,Co., Ltd.
Ningbo Fenghua Bolong Machinery Manufacturing Co., Ltd. is one of the most professional heat treatment manufacturers and suppliers in China, also supports high quality customized service. With abundant experience, we warmly welcome you to buy durable heat treatment made in China here from our factory.
Address: No. 27 Hehai Road, Binhai New Area, Fenghua Economic Development Zone, Ningbo City, Zhejiang Province
E-mail: sales@nbbolong.com
WebSite: https://www.nbbolongmachinery.com/